An R-on-1 laser-induced damage-threshold (LIDT) testing method was applied to test coated and uncoated magnesium oxide-doped periodically poled lithium niobate samples pumped by femtosecond Yb:KGW laser pulses at kilohertz and megahertz pulse repetition rates. LIDT values decreased by ∼1.5 and ∼38 times when increasing repetition rate from 100 to 571 kHz and to 76 MHz, respectively. We also investigated nonlinear absorption changes in lithium niobate crystals at the pulse repetition range from 60 to 600 kHz with trains consisting of 100 identical femtosecond pulses. Laser beam transmission in the crystal experienced a drop of ∼18 % from initial pulses of train to the next 40 pulses at intensities 40% to 15% lower than LIDT due to nonlinear absorption of 220 fs duration pulses at 1.03 μm.
We present experimental data obtained during investigation of synchronously pumped optical parametric oscillators (SPOPO’s) pumped by fundamental (1030 nm) and second harmonic (515 nm) radiation of mode-locked Yb:KGW laser, providing 105 fs pulses at 76 MHz repetition rate with an average power of 4 W. Different nonlinear crystals such as beta barium borate (BBO), and periodically poled lithium niobate (PPLN) and MgO doped PPLN (MgO:PPLN) were tested to estimate wavelength tuning capabilities and SPOPO’s efficiency. Rotation of BBO nonlinear crystal and SPOPO’s cavity length variation and, in the case of SPOPO based on PPLN, change of grating period and cavity length allowed signal wavelength tuning in 630 – 1030 nm and 1350 – 1700 nm spectral ranges, respectively. Parametric light conversion from pump power to signal power efficiency was as high as 25 %. Including the idler pulses the tuning ranges were from 630 to 2400 nm and from 1350 to 4000 nm in case of BBO and PPLN crystals, respectively. SPOPO based on BBO wsithout intracavity group velocity dispersion (GVD) compensation generates longer than transform limited pulses, so SPOPO based on BBO with dispersive prisms were investigated.
We report laser-induced damage threshold (LIDT) measurements of periodically poled lithium niobate (PPLN) and
magnesium-oxide-doped PPLN (MgO:PPLN) in the femtosecond pulse duration regime at 1030 nm with 100 kHz and 75
MHz repetition rate. PPLN and MgO:PPLN crystals with broadband Nb2O5/SiO2 AR coatings for 1.4 - 1.8 um spectral
range were used. S-on-1 test for LIDT measurements were performed. S was equal to 106 and 4.56*1010 pulses for 100
kHz CPA laser system and 75 MHz oscillator, respectively. Evaluated LIDT was 20 mJ/cm2 for 290 fs pulses at 100 kHz repetition rate and 0.63 mJ/cm2 for 105 fs pulses at 76 MHz repetition rate.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
INSTITUTIONAL Select your institution to access the SPIE Digital Library.
PERSONAL Sign in with your SPIE account to access your personal subscriptions or to use specific features such as save to my library, sign up for alerts, save searches, etc.