1 March 1994 Initiation of stress corrosion cracking of Ti90-Al6-V4 wire in aqueous solution by holometry
Author Affiliations +
Abstract
A study on stress corrosion cracking (SCC) of Ti90-AL6-V4 wire in anhydrous methanol has been conducted. The study focused on developing a relationship between microscopic deformation and corrosion current density in the incubation period of the SCC of the wire. The study succeeded in non-destructively monitoring the initiation stage of SCC by holographic interferometry `Holometry'. The monitoring process was carried out in situ applying the real-time holographic interferometry. In the mean time, the corrosion current density was determined by typical methods of electrochemistry. Consequently, a relationship between the influence of microscopic deformations on the corrosion current density is established.
© (1994) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Khaled J. Habib "Initiation of stress corrosion cracking of Ti90-Al6-V4 wire in aqueous solution by holometry", Proc. SPIE 2004, Interferometry VI: Applications, (1 March 1994); https://doi.org/10.1117/12.172601
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Corrosion

Holographic interferometry

Interferometry

Holography

Resistance

Electrodes

Hydrogen

Back to Top