Regarding its ability to circumvent the autofluorescence signal, persistent luminescence was recently shown to be a powerful tool for in vivo imaging and diagnosis applications in living animal. The concept was introduced with lanthanide-doped persistent luminescence nanoparticles (PLNP), from a lanthanide-doped silicate host Ca0.2Zn0.9Mg0.9Si2O6:Eu2+, Mn2+, Dy3+ emitting in the near-infrared window. In order to improve the behaviour of these probes in vivo and favour diagnosis applications, we showed that biodistribution could be controlled by varying the hydrodynamic diameter, but also the surface charges and functional groups. Stealth PLNP, with neutral surface charge obtained by polyethylene glycol (PEG) coating, can circulate for longer time inside the mice body before being uptaken by the reticulo-endothelial system. However, the main drawback of this first generation of PLNP was the inability to witness long-term monitoring, mainly due to the decay kinetic after several decades of minutes, unveiling the need to work on new materials with improved optical characteristics. We investigated a modified silicate host, diopside CaMgSi2O6, and increased its persistent luminescence properties by studying various Ln3+ dopants (for instance Ce, Pr, Nd, Tm, Ho). Such dopants create electron traps that control the long lasting phosphorescence (LLP). We showed that Pr3+ was the most suitable Ln3+ electron trap in diopside lattice, providing optimal trap depth, and resulting in the most intense luminescence decay curve after UV irradiation. A novel composition CaMgSi2O6:Eu2+,Mn2+,Pr3+ was obtained for in vivo imaging, displaying a strong near-infrared persistent luminescence centred on 685 nm, allowing improved and sensitive detection through living tissues.
© (2012) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Thomas Maldiney, Aurélie Lecointre, Bruno Viana, Aurélie Bessière, Didier Gourier, Michel Bessodes, Cyrille Richard, and Daniel Scherman "Trap depth optimization to improve optical properties of diopside-based nanophosphors for medical imaging", Proc. SPIE 8263, Oxide-based Materials and Devices III, 826318 (29 February 2012); https://doi.org/10.1117/12.909865
Lens.org Logo
CITATIONS
Cited by 8 scholarly publications.
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Luminescence

In vivo imaging

Nanoparticles

Ultraviolet radiation

Liver

Optical properties

Silicates

Back to Top