Porous graphite plates, cylinders and cones with densities of 1.55-1.82 g/cm3 were irradiated by a 10 kW fiber laser at 0.075 –3.525 kW/cm2 for 120 s to study mass removal and crater formation. Surface temperatures reached steady state values as high as 3767 K. The total decrease in sample mass ranged from 0.06 to 6.29 g, with crater volumes of 0.52 - 838 mm3, and penetration times for 12.7 mm thick plates as short as 38 s. Minor contaminants in the graphite samples produced calcium and iron oxide to be re-deposited on the graphite surface. Significantly increased porosity of the sample is observed even outside of the laser-irradiated region. Total mass removed increases with deposited laser energy at a rate of 4.83 g/MJ for medium extruded graphite with an apparent threshold of 0.15 MJ. Visible emission spectroscopy reveals C2 Swan and CN red, CN violet bands and Li, Na, and K 2P3/2,1/2 – 2S1/2 doublets. The reacting boundary layer is observed using a mid-wave imaging Fourier transform spectrometer (IFTS) at 2 cm-1 spectral resolution, 0.5 mm/pixel spatial resolution, and 0.75 Hz data cube rate. A two-layer radiative transfer model was used to determine plume temperature, CO, and CO2 concentrations from spectral signatures. The new understanding of graphite combustion and sublimation during laser irradiation is vital to the more complex behavior of carbon composites.
The various effects of laser heating of carbon materials are key to assessing laser weapon effectiveness. Porous graphite plates, cylinders, and cones with densities of 1.55 to 1.82 g/cm3 were irradiated by a 10-kW fiber laser at 0.075 to 3.525 kW/cm2 for 120 s to study mass removal and crater formation. Surface temperatures reached steady state values as high as 3767 K. The total decrease in sample mass ranged from 0.06 to 6.29 g, with crater volumes of 0.52 to 838 mm3, and penetration times for 12.7-mm-thick plates as short as 38 s. Minor contaminants in the graphite samples produced calcium and iron oxide to be redeposited on the graphite surface. Dramatic graphite crystalline structures are also produced at higher laser irradiances. Significantly increased porosity of the sample is observed even outside the laser-irradiated region. Total mass removed increases with deposited laser energy at a rate of 4.83 g/MJ for medium extruded graphite with an apparent threshold of 0.15 MJ. At ∼3.5 kW/cm2, the fractions of the mass removed from the cylindrical samples in the crater, surrounding trench, and outer region of decreased porosity are 38%, 47%, and 15%, respectively. Graphite is particularly resistant to damage by high power lasers. The new understanding of graphite combustion and sublimation during laser irradiation is vital to the more complex behavior of carbon composites.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
INSTITUTIONAL Select your institution to access the SPIE Digital Library.
PERSONAL Sign in with your SPIE account to access your personal subscriptions or to use specific features such as save to my library, sign up for alerts, save searches, etc.